Powder coating
Powder coating runs a part through a phosphate or blast prep, a spray.
Open15 August 2026
Powder coat colour matching across a reorder is unreliable beyond about eighteen months, because the powder batch changes and the cure line drifts.
On a large flat surface the difference reads as a mismatch, and on a frame it reads as a slightly different chair. Reserving powder for a later order is possible and rarely done. Railings and other long runs are where colour drift shows most, because the eye compares one length against the next.
The warranty claim on a colour matched at year two usually ends with a full recoat, so the cheaper route is to hold a powder batch reference at the first order.
Moisture content decides everything a timber frame will do later. At 8 to 12 percent, stock stays where it was machined. At 15 percent it shrinks across the grain and opens joints that were tight in the workshop. Coating thickness on powder is measured in microns and quoted in colours.
At 60 to 80 microns the film survives a service trolley. At 40 it chips at the first contact and rust starts in the chip.
Aluminium does not rust and does not take a weld the way steel does. In a load-bearing frame that difference is structural. Cosmetic variation costs nothing to live with, and this does. Heat and grease attack finishes from the underside, where cleaning never goes. The underside of a table apron in a grill room is the first place a coating fails.
Stain colour drifts between batches of the same species. Ten frames stained in March and twenty in July will read as two different colours unless the stain lot is held. Species, section size, moisture content and coating thickness are four lines that determine how a frame ages. Leave any of them out and the factory will choose, usually for cost.
The finish on a chair leg takes more knocks than any other surface in the dining area. Two coats on the legs and one on the rails is a false economy that shows in year two. The visible difference between a good frame and a cheap one is often at the back, where nobody looks until it fails. Ask for a photograph of the reverse side. Every model sits inside the steakhouse range.
Rubberwood is a plantation timber with a short rotation, which shows in the density. At 600 kg per cubic metre it holds a screw and takes a finish, and it dents under a chair leg where beech would not. Quarter sawn stock is stable and expensive, and flat sawn is the reverse. The quarter sawn leg moves 2 mm across its width where the flat sawn leg moves 6 mm, which is the whole argument for the price.
Brass is a wear surface in a steakhouse. The lacquered brass foot rail holds its colour for two years and then goes patchy. The unlacquered rail patinas evenly and needs polishing if the dining area wants shine. Welds on a coated frame need cleaning before the coating goes on. Cleaning afterwards means stripping the coat back. The weld left with spatter reads as a lump under 70 microns of powder, and the lump is where the coat cracks first. Booth geometry is set out under leather booth seating.
Yes, and the frame has to be stripped first, which costs about a third of a new frame.
Powder coating runs a part through a phosphate or blast prep, a spray.
OpenFurniture welding is usually MIG at 3 to 4 mm fillet, and the failure point is the toe rather than the throat.
OpenRecovering half the floor creates a colour problem instead of a wear problem.
OpenSpecies, moisture, wall thickness, coating and how each one ages in a grill room.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.