Steel or aluminium
Steel and aluminium frames differ in stiffness, weight and repairability.
Open3 August 2026
Furniture welding is usually MIG at 3 to 4 mm fillet, and the failure point is the toe instead of the throat.
The weld that has been ground flush removes the toe that carries the load. The frame inspected on the outside of the joint tells you nothing, because the crack starts on the inside face. The weld cooled too fast is harder than the tube around it, and the crack then runs into the parent metal instead of staying in the joint.
Tube joints that are coped before welding fit without a gap, and a gap of 1 mm halves the fatigue life of the joint.
Wall thickness in steel tube is the number that gets hidden. At 1.5 mm a frame dents at the first knock. At 2.0 mm the same section takes the knock and rings differently when it is tapped. Aluminium does not rust and does not take a weld the way steel does.
In a load-bearing frame that difference is structural. Cosmetic variation costs nothing to live with, and this does.
Solid timber moves, plywood does not. The solid top on a plywood carcass is a joint that opens. The same top on a solid frame moves with the carcass and stays closed. Welds fail at the toe, where the heat affected zone meets parent metal. The weld that looks smooth can have a toe crack that appears after a thousand flexing cycles.
Species, section size, moisture content and coating thickness are four lines that determine how a frame ages. Leave any of them out and the factory will choose, usually for cost. Ask for the moisture reading at dispatch. Timber takes up water between the two dates. The frame that leaves the workshop at 9 percent and arrives at 14 has spent a month in a container getting wet.
Corrosion starts at fixings. Stainless screws into a steel frame with no barrier is a galvanic couple that fails before the coating does.
Veneer is a surface. It needs a substrate that will not move. The 0.6 mm walnut veneer on an 18 mm plywood core stays flat. The same veneer on particle board telegraphs every joint through the face. Sizes, finishes and lead times are set out across steakhouse seating.
Finger jointing is how short lengths become a rail. The joint at 10 mm fingers holds in bending and shows as a line under a clear finish, which is a look instead of a fault. Welds on a coated frame need cleaning before the coating goes on. Cleaning afterwards means stripping the coat back. The weld left with spatter reads as a lump under 70 microns of powder, and the lump is where the coat cracks first.
Screw grade decides whether a fixing survives a wet dining area. The A2 stainless screw into a steel frame holds. The zinc plated screw at the same size rusts at the head inside a year and stains the timber around it. Relative humidity in a dining room sits between 40 and 60 percent, and the furniture is built for it. The dining area run at 25 percent in winter moves every solid top and opens every joint that was tight at handover. Depths and back angles sit under leather steakhouse booths.
On a painted frame, a dressed weld reads as a smooth joint. On a powder coated frame, a ground toe is a stress riser, so leaving the weld visible is often stronger.
Steel and aluminium frames differ in stiffness, weight and repairability.
OpenSteel tube thickness in furniture runs 1.2 to 2.5 mm, and the number is rarely quoted.
OpenFurniture quality claims settle on evidence, and evidence is three things: the model code.
OpenSpecies, moisture, wall thickness, coating and how each one ages in a grill room.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.