Welding
Furniture welding is usually MIG at 3 to 4 mm fillet, and the failure point is the toe instead of the throat.
Open9 August 2026
Powder coating runs a part through a phosphate or blast prep, a spray, and a cure at 180 to 200 degrees for about 15 minutes.
The prep is what the film adheres to, so a part that was wiped instead of phosphated chips at the first knock. Film thickness of 60 to 80 microns is measured on the part. The test panel beside the rack does not show what a shielded leg gets. Rack marks are where the part touched the jig, and they appear as bare patches on a face that nobody checked.
Outgassing from a casting produces pinholes in a powder coat. That is why cast bases need a different prep from tube frames.
Beech machines cleanly and takes a screw without splitting. That is why it is the default for painted frames. Ash has a more open grain and a longer fibre, so it survives impact better and shows every coat.
Wall thickness in steel tube is the number that gets hidden. At 1.5 mm a frame dents at the first knock. At 2.0 mm the same section takes the knock and rings differently when it is tapped. Coating thickness on powder is measured in microns and quoted in colours.
At 60 to 80 microns the film survives a service trolley. At 40 it chips at the first contact and rust starts in the chip.
Heat and grease attack finishes from the underside, where cleaning never goes. The underside of a table apron in a grill room is the first place a coating fails. Stain colour drifts between batches of the same species. Ten frames stained in March and twenty in July will read as two different colours unless the stain lot is held.
Species, section size, moisture content and coating thickness are four lines that determine how a frame ages. Leave any of them out and the factory will choose, usually for cost. Powder coat colour matching across a reorder is unreliable beyond about eighteen months. The same RAL from a different batch reads slightly differently, and on a large flat surface that reads as a mismatch.
Steel and timber in the same frame need a barrier between them. Bare steel against damp timber rusts in a season, and the stain it leaves will not come out of a light cover. Rubberwood is a plantation timber with a short rotation, which shows in the density. At 600 kg per cubic metre it holds a screw and takes a finish, and it dents under a chair leg where beech would not. All 829 models are listed on the steakhouse furniture page.
Glue on end grain needs a size coat or it starves. The joint sized and left for ten minutes holds. The joint glued straight onto dry end grain pulls apart at the first dry season. Welds on a coated frame need cleaning before the coating goes on.
Cleaning afterwards means stripping the coat back. The weld left with spatter reads as a lump under 70 microns of powder, and the lump is where the coat cracks first.
Timber and steel in one frame move differently with temperature. The steel rail at 20 degrees and the timber seat at the same temperature part company by 1 mm over a 2 m run. That is why the fixing needs a slot. Runs are drawn up under custom booth seating.
Because the prep was skipped, the film was too thin, or the part was coated over a sharp edge. All three are visible at the chip instead of at the surface.
Furniture welding is usually MIG at 3 to 4 mm fillet, and the failure point is the toe instead of the throat.
OpenSteel and aluminium frames differ in stiffness, weight and repairability.
OpenFront legs at 32 mm square in beech carry a 150 kg static load with a 60 mm tenon and no visible deflection.
OpenSpecies, moisture, wall thickness, coating and how each one ages in a grill room.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.