Steel tube thickness in furniture runs 1.2 to 2.5 mm, and the number is rarely quoted.
At 1.5 mm a frame dents at the first knock and rings flat when tapped. At 2.0 mm the same section takes the knock and returns. Wall thickness also sets how much heat a weld can take before it burns through. Tapping a frame tells you the wall thickness: a thin tube rings flat and a thick one rings with a note.
Tube thickness matters most at the footrest of a stool and the arm of a chair, which are the two places a body lands.
Coating thickness on powder is measured in microns and quoted in colours. At 60 to 80 microns the film survives a service trolley. At 40 it chips at the first contact and rust starts in the chip. Aluminium does not rust and does not take a weld the way steel does.
In a load-bearing frame that difference is structural. Cosmetic variation costs nothing to live with, and this does.
Species, section size, moisture content and coating thickness are four lines that determine how a frame ages. Leave any of them out and the factory will choose, usually for cost. Steel and timber in the same frame need a barrier between them. Bare steel against damp timber rusts in a season, and the stain it leaves will not come out of a light cover.
Corrosion starts at fixings. Stainless screws into a steel frame with no barrier is a galvanic couple that fails before the coating does. Repair on timber is straightforward if the section is thick enough to take a plug. Below about 40 mm square there is no material left to repair into, and the part gets replaced.
Rubberwood is a plantation timber with a short rotation, which shows in the density. At 600 kg per cubic metre it holds a screw and takes a finish, and it dents under a chair leg where beech would not.
Veneer is a surface. It needs a substrate that will not move. The 0.6 mm walnut veneer on an 18 mm plywood core stays flat. The same veneer on particle board telegraphs every joint through the face.
Salt spray hours are the only comparable corrosion number. The 200 hour coating survives a coastal dining area. The 48 hour coating at the same colour fails at the weld in one season. Welds on a coated frame need cleaning before the coating goes on. Cleaning afterwards means stripping the coat back. The weld left with spatter reads as a lump under 70 microns of powder, and the lump is where the coat cracks first. Quotations start from the Ember & Chair range.
Timber and steel in one frame move differently with temperature. The steel rail at 20 degrees and the timber seat at the same temperature part company by 1 mm over a 2 m run. That is why the fixing needs a slot.
Screw grade decides whether a fixing survives a wet dining area. The A2 stainless screw into a steel frame holds. The zinc plated screw at the same size rusts at the head inside a year and stains the timber around it. Runs are drawn up under custom booth seating.
By weight and by tapping. The 2.0 mm frame is noticeably heavier in the hand than a 1.5 mm one of the same shape, and it sounds different.
Plywood and MDF are the two cores behind most upholstered furniture, and they fail differently.
OpenWalnut veneer at 0.6 mm gives a species that would be too expensive in solid form, and it cannot be sanded at all.
OpenKnock-down packing trades container space for assembly and for joints.
OpenSpecies, moisture, wall thickness, coating and how each one ages in a grill room.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.
Own workshop · EXW Foshan or DDP
Send the plan and the seat count. Answer inside two working days.
Chat on WhatsApp