Ember & Chair Steakhouse seating · Foshan, China WhatsApp
Send the floor plan and the seat count. Layout and quote back in two working days. Talk to us →
Steakhouse furniture Ember & ChairSteakhouse seating 829 models Design
Home/Blog/Cracking

Cracks appear along folds. The fold is where the surface flexes, and flexing is what breaks a finish.

Leather cracking starts at a fold line, because that is where the surface flexes rather than abrades.

Fold line
flex failure
Front edge
abrasion or finish failure
Back
heat and dryness

Grain, finish and thickness

The crack at the seat front edge is usually a finish failure on a pigmented hide. The crack across the back is usually dryness from heat. Both look like the same problem and have different causes. Heat from a grill dries the finish from the inside, so a back two metres from a fire cracks before the seat does.

Cleaning with a solvent strips the finish that protects the hide, and the patch cleaned weekly becomes the patch that cracks first.

Heat, grease and dye

Heat is what kills covers in a steakhouse, and it kills them from behind. The back of a booth two metres from a grill reaches temperatures that dry the finish from the inside out. PU at 1.2 mm is a coated split with its own failure mode. It cleans better, it does not patina, and it delaminates instead of cracks.

Inside two metres of a fire, the cover has to change. Inside it, hide needs a fire-retardant treatment or a different cover altogether. Fire treatment changes the hand of a hide. Treated stock sits stiffer and creases along different lines, which matters on a curved back where the cover has to follow the shape.

The line on the order

Surface wear in a steakhouse is concentrated on the seat front edge and the booth back at shoulder height. Those two zones take about 80 percent of the abrasion in a dining area. Hide is sold by area and cut by shape, so the yield is a layout question. The average hide at 4.5 square metres yields 12 seat covers if the arms are cut from the belly and 9 if the back is cut from a single piece.

Thickness varies across one hide by up to 0.3 mm. The cover cut from the shoulder takes a harder wear line than the same cover cut from the flank, and no specification catches it. Thread fails before hide does in most covers. The polyester at 40/3 holds a seam under tension. The cotton thread rots at the needle holes and the seam opens along the stitch line. All 829 models are listed on the steakhouse furniture page.

How to check it on a sample

Cold dining areas and hot dining areas age hide differently. The space at 18 degrees and 50 percent humidity keeps a hide supple for a decade. The space at 26 degrees dries it from the back and cracks at every fold. Webbing and foam under a cover matter as much as the cover.

The seat webbed at 8 percent tension holds a hide flat. The loose web lets the hide fold at the front edge and the fold cracks first.

Deep cleaning on hide belongs on a schedule. The reaction cleans too late and cleans too hard. The quarterly clean with a pH neutral product keeps a cover. The annual scrub with a solvent takes the finish off and calls it cleaning. Re-covering a chair uses less hide than the original, which changes the cost of a refurb. The second cover needs 0.9 square metres where the first took 1.2, because the panels are already cut to size. Every upholstered stool is listed under steakhouse counter stools.

One more question

Can cracking be stopped?

Slowed, by conditioning and by keeping heat away. The crack that has started does not close, and the repair is a patch or a recover.

Stretching

Leather stretches 3 to 8 percent under a stretched cover.

Open

Colour matching

Leather colour matching usually fails because the light is different. Two drums of the same dye read apart under a window and together under a warm pendant.

Open

Verification

The order for 120 seats can pass through four hands before a saw is switched on: the one that sells.

Open

Hide and covers

Grain, thickness, dye lots, cleaning and the two metres around a fire.

Open

Send the floor plan. Get the layout and the quote.

Dimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.

Own workshop · EXW Foshan or DDP

Design referencesFourteen positions, measured→ Buying guidesEight decisions, with the numbers→ BlogThree hundred notes, two a day→ Project filesThree projects, and what changed→ The spec sheetNine numbers and the tolerance→ Talk about your steakhouseSend the plan, get a seat count→