Leather grades
Leather grading runs from full grain through top grain to corrected grain.
Open30 June 2026
Full grain and top grain differ by how much of the outer surface was sanded before finishing.
Full grain keeps the whole surface, including scars and insect marks, and darkens with use. Top grain has had 0.2 to 0.5 mm removed, which makes it more uniform. At the same thickness it also wears through sooner. Full grain develops a patina that reads as quality at year three and as tired at year eight, and the same process produces both.
Top grain takes a pigment finish more evenly. That is why it dominates in dining areas that need colour consistency across hundreds of seats.
Thickness is the first number and the least understood. At 1.4 mm a corrected hide takes the abrasion of a booth back and still bends round a corner radius. At 1.8 mm it lasts longer and will not follow a tight turn without pleating.
Grain is a surface finish. Grade is a separate scale. Corrected grain hides are sanded flat and embossed, which makes them uniform and removes the surface that would have shown wear most gracefully.
Colour under 2700 K tungsten reads warmer than under 4000 K retail lighting. Swatches approved in a showroom get approved in the wrong dining area, which is a delay dressed as a defect.
The sample has to prove thickness and backing. Colour is the easy part. The 100 mm swatch shows the colour and hides everything else that decides how the cover behaves on a seat.
Cost per square metre is not cost per seat. Cutting yield on a hide varies by 15 to 20 percent depending on the panel shapes, so two quotes at the same price per metre can differ by a fifth per seat. Thickness varies across one hide by up to 0.3 mm. The cover cut from the shoulder takes a harder wear line than the same cover cut from the flank, and no specification catches it.
Leather has a stretch direction, exactly like timber has a grain. The cover cut with the stretch running across the seat takes the load. The cover cut against it sags at the front edge. Hydrolysis is what kills PU, and it is a climate question. The PU specified for a humid coastal dining area needs a hydrolysis resistant grade, and the standard grade fails at year three with a sticky surface. All 829 models are listed on the steakhouse furniture page.
Cold dining areas and hot dining areas age hide differently. The space at 18 degrees and 50 percent humidity keeps a hide supple for a decade. The space at 26 degrees dries it from the back and cracks at every fold. Seats and backs want different leather. The seat takes abrasion and grease, the back takes pressure and friction, and using the heavier hide on the back spends money where it does not wear.
Deep cleaning on hide belongs on a schedule. The reaction cleans too late and cleans too hard. The quarterly clean with a pH neutral product keeps a cover. The annual scrub with a solvent takes the finish off and calls it cleaning.
The colour pen covers a scratch. On a crack it shows as a darker line. The pen matched to the dye lot hides a scuff at handover. The same pen on a cracked finish shows as a darker line within a month. Footrest and ledge heights sit under high top stools.
It is better on a seat that will be treated well. On a run where colour consistency matters across 60 seats, top grain wins by not showing the difference.
Leather grading runs from full grain through top grain to corrected grain.
OpenLeather sample approval should cover thickness, backing, hand and colour.
OpenThe claim window is set by the contract and shortened by use.
OpenGrain, thickness, dye lots, cleaning and the two metres around a fire.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.