Ember & Chair Steakhouse seating · Foshan, China WhatsApp
Send the floor plan and the seat count. Layout and quote back in two working days. Talk to us →
Steakhouse furniture Ember & ChairSteakhouse seating 829 models Design
Home/Blog/Welds

The weld that looks smooth can carry a crack at the toe.

Welds on a steel chair frame fail at the toe, where the heat affected zone meets parent metal.

Failure point
weld toe, heat affected zone
Wall
1.5 to 2.0 mm
Check
inside of the joint

Load paths through a seat

The weld that looks smooth can carry a toe crack that opens after a thousand flexing cycles, and the crack starts on the inside of the joint where nobody looks. Visible weld size is a poor guide to whether it will hold. Grinding a weld flush removes the toe that carries the load. That is why a smoothed joint is often weaker than a visible one.

Tube wall thickness sets how much heat a weld can take: 1.5 mm wall burns through before 2.0 mm reaches penetration. The weld cooled too fast is harder than the tube around it, and the crack then runs into the parent metal rather than staying in the joint.

The failure nobody sees

The underside is where a frame tells the truth. Corner blocks, staple rows and the way a rail meets a leg show in one photograph whether the joint was cut or assembled from a kit. The screw into end grain holds about 400 N in a test and less every time it is turned. Once the thread is gone the rail needs a dowel plug before it will take another one.

Welded steel and glued timber fail differently. Steel cracks at the weld toe after repeated flexing. Timber creeps at the glue line. Neither announces itself before it happens.

What the drawing should say

Ask what happens at the third repair. One repair tells you nothing. Any frame survives one repair. The question is whether the leg still has timber left to take a wedge.

Tenon thickness should be a third of the rail it sits in. The 22 mm tenon in a 70 mm rail leaves 24 mm of timber each side, which is what stops the mortise cheek breaking out under a side load. Clamp pressure for a PVA joint is 0.5 to 1 N per square millimetre and it needs 30 minutes before the clamp comes off. The chair assembled and unclamped after five minutes fails at the same tenon in the same year.

Weld size on a steel frame is measured at the leg. The flat is where the weld is easiest to run and least likely to fail. The 4 mm fillet that looks generous in a photograph is a 2.5 mm throat once measured, and that is the number that decides fatigue life. Weld penetration matters at the seat rail, where the bending moment peaks. The tack welded rail looks finished and fails inside two years of drag load, because a tack carries no bending at all. Every model sits inside the steakhouse range.

How to check it on a sample

Leg section is a stiffness number before it is a style number. Going from 32 mm square to 28 mm square removes 40 percent of the second moment of area, and the chair that looked slender at the sample stage starts to flex in service. Test to the load the dining area will produce. The 150 kg static test with no cycle count says nothing about a chair dragged four times a night for ten years.

Repair is limited by the timber left around the mortise. The tenon re-cut inside a mortise wall thinned by one repair has one more repair in it, and the second one is where the cheek splits. Foam wrapping is a wear decision. The 20 mm wrap that covers the foam edge stops the cover abrading on the frame rail. The unwrapped edge rubs through at the front corner inside three years. Capacity and lead times are explained on the Ember & Chair workshop.

One more question

Should welds be ground smooth?

Only cosmetically, and never at the toe. The ground toe is a stress riser on a part that already flexes.

Coating

Powder coat at 60 to 80 microns survives a service trolley and a chair dragged across a tiled floor.

Open

Moisture content

Timber at 8 to 12 percent moisture content stays where it was machined in a conditioned dining area.

Open

Top thickness

Table top thickness at 25 mm over a base spread of 600 mm stays flat under a leaning guest.

Open

Chair frames

Joints, glue lines, foam and the parts of a chair that decide year eight.

Open

Send the floor plan. Get the layout and the quote.

Dimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.

Own workshop · EXW Foshan or DDP

Design referencesFourteen positions, measured→ Buying guidesEight decisions, with the numbers→ BlogThree hundred notes, two a day→ Project filesThree projects, and what changed→ The spec sheetNine numbers and the tolerance→ Talk about your steakhouseSend the plan, get a seat count→