Blackened steel
Blackened steel is chemically treated instead of coated, so the colour is in the surface instead of on it.
Open14 October 2026
Reclaimed timber brings character, unknown moisture content and embedded metal.
The single nail through a planer head costs more than the timber saved, and metal detection on every board is the only control. Reclaimed stock also arrives at a moisture content that has to be brought down before machining. Reclaimed boards vary in thickness after cleaning up, so a top built from them ends up thinner than the drawing.
Old timber is often more stable than new, because it has already moved, which is the one real advantage.
Moisture content decides everything a timber frame will do later. At 8 to 12 percent, stock stays where it was machined. At 15 percent it shrinks across the grain and opens joints that were tight in the workshop. Welds fail at the toe, where the heat affected zone meets parent metal. The weld that looks smooth can have a toe crack that appears after a thousand flexing cycles.
Reclaimed timber carries a story and a risk. Nails, grit and unknown moisture all live inside it, and one nail through a planer head costs more than the timber saved. Species, section size, moisture content and coating thickness are four lines that determine how a frame ages. Leave any of them out and the factory will choose, usually for cost.
Ask for the moisture reading at dispatch. Timber takes up water between the two dates. The frame that leaves the workshop at 9 percent and arrives at 14 has spent a month in a container getting wet. Timber bought for a grill room should be dried for the climate it is going to. The frame dried to European winter and shipped to a humid coastal dining area will take up moisture on arrival.
Veneer is a surface. It needs a substrate that will not move. The 0.6 mm walnut veneer on an 18 mm plywood core stays flat. The same veneer on particle board telegraphs every joint through the face.
Insect attack in imported timber is a documentation and a kiln question. The stock kiln dried to 60 degrees for four hours is dead. The stock dried at 50 degrees can carry larvae into a building. Moisture readings are taken at three places on a rail. One reading on one rail says nothing about the batch. The end grain reads 2 to 3 percent wetter than the middle of the same board, and the end grain is where the joint is. Every model sits inside the steakhouse range.
Quarter sawn stock is stable and expensive, and flat sawn is the reverse. The quarter sawn leg moves 2 mm across its width where the flat sawn leg moves 6 mm, which is the whole argument for the price. Fumed and smoked colours come from a reaction with the timber itself. Ammonia fuming on oak darkens through the timber and cannot chip. The stain that copies it sits on the surface and wears through at the edge.
Anodising on aluminium is a thickness and a sealing question. The 15 micron anodised leg resists a wipe down. The 8 micron anodised leg goes chalky in a year of cleaning. Depths and back angles sit under leather steakhouse booths.
Rarely, once the cleaning, detecting and machining are counted. It is a design choice instead of a saving.
Blackened steel is chemically treated instead of coated, so the colour is in the surface instead of on it.
OpenBrass accents on furniture are either solid, plated or lacquered, and each ages differently.
OpenMicrofiber seating uses a fine synthetic fibre with a suede-like surface.
OpenSpecies, moisture, wall thickness, coating and how each one ages in a grill room.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.
Own workshop · EXW Foshan or DDP
Send the plan and the seat count. Answer inside two working days.
Chat on WhatsApp