Semi-aniline
Semi-aniline leather has a light pigment coat over an aniline base, typically 5 to 20 microns.
Open24 July 2026
Pigmented leather carries a pigment and a protective top coat, typically 25 to 50 microns total, which makes it uniform, cleanable and resistant.
It also means the surface that wears is a coating instead of the hide, so failure looks like a crack or a peel instead of a gradual softening. It is the standard choice for high-traffic seating. Pigmented hides clean with a damp cloth and survive a wine spill, which is the practical reason they dominate in dining areas that serve alcohol with the meal.
The pigmented coat that cracks has failed from flexing instead of from abrasion, so the crack appears along a fold line and not where the seat is used most.
Grain is a surface finish. Grade is a separate scale. Corrected grain hides are sanded flat and embossed, which makes them uniform and removes the surface that would have shown wear most gracefully.
PU at 1.2 mm is a coated split with its own failure mode. It cleans better, it does not patina, and it delaminates instead of cracks. Aniline and semi-aniline absorb. In a steakhouse that means a wine spill is permanent in a way it is not on a pigmented hide, and the dining area has to be specified around that fact.
Fire treatment changes the hand of a hide. Treated stock sits stiffer and creases along different lines, which matters on a curved back where the cover has to follow the shape. Repair on hide is possible and often invisible. On PU it is neither, which is the hidden cost of the cheaper cover at the point where the dining area needs fixing instead of replacing.
Leather has a stretch direction, exactly like timber has a grain. The cover cut with the stretch running across the seat takes the load. The cover cut against it sags at the front edge. Stitch length is a strength decision.
Eight stitches per inch closes a seam that holds. Twelve stitches per inch cuts the hide along the needle line like a perforation.
Backing cloth decides whether PU survives a hot dining area. The knitted backing at 120 g per square metre holds the coating flat. The non-woven backing delaminates at the seat front where the flexing happens. Cold dining areas and hot dining areas age hide differently. The space at 18 degrees and 50 percent humidity keeps a hide supple for a decade. The space at 26 degrees dries it from the back and cracks at every fold. Sizes, finishes and lead times are set out across steakhouse seating.
Webbing and foam under a cover matter as much as the cover. The seat webbed at 8 percent tension holds a hide flat. The loose web lets the hide fold at the front edge and the fold cracks first. Seats and backs want different leather. The seat takes abrasion and grease, the back takes pressure and friction, and using the heavier hide on the back spends money where it does not wear.
The colour pen covers a scratch. On a crack it shows as a darker line. The pen matched to the dye lot hides a scuff at handover. The same pen on a cracked finish shows as a darker line within a month. Every upholstered stool is listed under steakhouse counter stools.
Pigmented, on a run where guests lean back after a meal. The coating takes the grease that an aniline would absorb.
Semi-aniline leather has a light pigment coat over an aniline base, typically 5 to 20 microns.
OpenAniline leather is dyed through and left unfinished, so the surface is the hide itself.
OpenDaily cleaning of steakhouse seating is a dry cloth followed by a damp one, in that order.
OpenGrain, thickness, dye lots, cleaning and the two metres around a fire.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.
Own workshop · EXW Foshan or DDP
Send the plan and the seat count. Answer inside two working days.