Abrasion
Fabric abrasion is measured in double rubs on a Wyzenbeek or Martindale machine.
Open22 October 2026
Double rub count measures a back and forth movement as a single cycle. That is why a 15,000 double rub fabric has taken 15,000 cycles rather than 30,000 rubs.
The number is a comparison between fabrics tested the same way, and it is not a prediction of years. The seat that is entered four times an hour takes more abrasion in a week than a sofa takes in a year. Test results are quoted at the point where two yarns break, which is a defined failure instead of the point where a fabric looks worn.
The fabric that passes at 30,000 double rubs can still fail at a seam in the first year, because the seam is not what the test measures.
Thickness is the first number and the least understood. At 1.4 mm a corrected hide takes the abrasion of a booth back and still bends round a corner radius. At 1.8 mm it lasts longer and will not follow a tight turn without pleating. Grease is the second enemy after heat, and it works on the underside and the seams. The cover that looks clean can be holding a film of fat in the stitch line that slowly softens the thread.
Seams are where a cover fails first in a booth, because the seam sits at the entry point and takes the abrasion of every slide-in. Cost per square metre is not cost per seat. Cutting yield on a hide varies by 15 to 20 percent depending on the panel shapes, so two quotes at the same price per metre can differ by a fifth per seat.
Patina is a selling point until it becomes a complaint. Full grain darkens and softens in a way that reads as quality at year three and as tired at year eight, and the same process produces both. Hide is sold by area and cut by shape, so the yield is a layout question. The average hide at 4.5 square metres yields 12 seat covers if the arms are cut from the belly and 9 if the back is cut from a single piece.
The spine is the firmest part of a hide and the belly the loosest. Covers cut with the back panel from the spine and the seat from the belly hold shape. The reverse gives a back that wrinkles in a season. Coating adhesion is the number that predicts failure in a grill room. The finish bonded at under 3 N per centimetre lifts at the seam within two years of heat and wipe down. Sizes, finishes and lead times are set out across steakhouse seating.
Abrasion is quoted in Martindale cycles and read in the wrong context. The 50,000 cycle hide and the 25,000 cycle PU both survive a steakhouse for five years, because nothing in the dining area abrades for 25,000 cycles. Hydrolysis is what kills PU, and it is a climate question. The PU specified for a humid coastal dining area needs a hydrolysis resistant grade, and the standard grade fails at year three with a sticky surface.
Armrests and seat fronts take the hardest wear in a dining area. The cover specified for a back panel is fine on the back and gone in two years on an armrest that hands rest on. Ultraviolet through a window fades the window side first. The covers rotated between window and wall seats at year two keep an even dining area. The ones left in place do not. Every upholstered stool is listed under steakhouse counter stools.
Contract grade at 30,000 double rubs, on a fabric that also resists oil. The second condition eliminates more options than the first.
Fabric abrasion is measured in double rubs on a Wyzenbeek or Martindale machine.
OpenMicrofiber seating uses a fine synthetic fibre with a suede-like surface.
OpenTimber warps when one face takes up moisture faster than the other.
OpenGrain, thickness, dye lots, cleaning and the two metres around a fire.
OpenDimensions, seat count and the finish you have in mind are enough to start. What comes back is a quantity per line, a leather card, a sample date and a loading window. All of it fits on one page.
Own workshop · EXW Foshan or DDP
Send the plan and the seat count. Answer inside two working days.
Chat on WhatsApp